Top-class zinc carries a premium, so the sensible question is where it earns that premium and where it does not. The answer is not a matter of preference: in some processes the trace elements in a lower class cause a defect that appears long after delivery, and in others they are irrelevant. This post draws the line.

Application Map

ApplicationRecommended classReason
Zinc die-casting alloys99.995%Grain-boundary corrosion from Sn, Cd, Pb
Continuous galvanizing99.995%Bath chemistry control, dross management
High-purity zinc oxide99.995%Impurities carry into the oxide
Batch hot-dip galvanizing99.95% often sufficientBath tolerates wider trace range
Brass casting99.95% often sufficientAlloy additions dominate chemistry
Zinc anodesDepends on specificationStandard defines the class to use

The Die-Casting Case

Zinc die-casting alloys are the clearest case for the top class. Tin, cadmium and lead do not dissolve in the zinc matrix; they segregate at grain boundaries, where moisture creates an electrochemical cell. The part swells, loses dimensional tolerance and in severe cases cracks. The process takes months, so the defect reaches the customer before it becomes visible. Tin is the most aggressive of the three and its limit in the top class is ten times tighter than in the 99.95% class.

Where the Premium Does Not Pay

In brass casting, deliberate alloy additions dominate the final chemistry and the trace elements in a lower zinc class fall well within the alloy's own tolerance. In batch hot-dip galvanizing, bath chemistry is managed continuously and the bath itself tolerates a wider trace range; the quality of the coating depends far more on surface preparation and bath temperature control than on the last 0.045% of input zinc purity.

Deciding for Your Process

  • Does your part specification set a limit for lead, cadmium or tin?
  • Does your process produce a delayed failure mode, as die-casting does?
  • Do deliberate alloy additions dominate the final chemistry?
  • Has any past scrap or warranty claim been traced to input chemistry?
  • Is your end market subject to restricted-substance rules?

If the first two are yes, specify 99.995%. If the third is yes and the others no, a lower class is usually a sound commercial decision — made explicitly, with the trace limits still written into the order.

Can I mix classes in the same facility?
Yes, and many plants do: top class for the die-casting line, a lower class for general use. It requires separate storage areas and clear labelling, because a mix-up removes the benefit of buying the top class at all.
Does a higher class improve coating appearance in galvanizing?
Marginally at best. Coating appearance is governed by surface preparation, bath temperature, withdrawal rate and bath chemistry management. Input purity matters for dross formation and bath additive control, not for visual finish.
Is restricted-substance compliance a reason on its own?
It can be. Cadmium and lead appear in restricted-substance rules for several end markets, and the tighter limits of the top class make compliance easier to document. Check the rules your end market applies.
How do I verify the class on arrival?
Compare the per-lot CoA against your written limits, confirm cast and lot numbers match the shipment labels, and run independent spectrometric analysis on the first lots from a new supplier.
Atso Tek Zinc CatalogGrade tables, packaging options and shipping documents in one file.PDF ↓
/ Continue reading
STANDARDS
Nov 2026

SHG Zinc Ingot: What the Grade Name Actually Covers

Read article
GUIDE
Oct 2026

Primary vs secondary aluminum ingot: what changes for the buyer

Read article
GUIDE
Oct 2026

What is an aluminum ingot? A7 and A8 explained

Read article
Call WhatsAppGet quote